AWS B2.1-5A-226:2022, Standard Welding Procedure Specification (SWPS) for Gas Tungsten Arc Welding (Consumable Insert Root) Followed by Shielded Metal Arc Welding of Chromium- Molybdenum Steel (M-5A/P-5A), IN521, ER90S-B3, and E9018-B3, 1/8 Inch [3 Mm] Through 1/2 Inch [13 Mm] Thick, As-Welded Condition; 1/8 Inch [3 Mm] Through 1-1/2 Inch [38 Mm] Thick, PWHT Condition, Primarily Pipe Applications