The Relative Stress-corrosion-cracking Susceptibility of Candidate Aluminum-lithium Alloys for Aerospace Applications


Book Description

Stress corrosion tests of Al-Li-Cu powder metallurgy alloys are described. Alloys investigated were Al-2.6% Li-1.4% and Al-2.6% Li-1.4% Cu-1.6% Mg. The base properties of the alloys were characterized. Process, heat treatment, and size/orientational effects on the tensile and fracture behavior were investigated. Metallurgical and electrochemical conditions are identified which provide reproducible and controlled parameters for stress corrosion evaluation. Preliminary stress corrosion test results are reported. Both Al-Li-Cu alloys appear more susceptible to stress corrosion crack initiation than 7075-T6 aluminum, with the magnesium bearing alloy being the most susceptible. Tests to determine the threshold stress intensity for the base and magnesium bearing alloys are underway. Twelve each, bolt loaded DCB type specimens are under test (120 days) and limited crack growth in these precracked specimens has been observed. General corrosion in the aqueous sodium chloride environment is thought to be obscuring results through crack tip blunting.







Materials for Marine Systems and Structures


Book Description

Treatise on Materials Science and Technology, Volume 28: Materials for Marine Systems and Structures provides an integrated approach, utilizing the environmental information of the ocean scientists, materials science, and structural integrity principles as they apply to offshore structures and ships. The book discusses the materials and their performance in marine systems and structures; the marine environment; and marine befouling. The text also describes marine corrosion; corrosion control; metallic materials for marine structures; and concrete marine structures. Materials for mooring systems and fracture control for marine structures are also considered. Professional scientists and engineers, as well as graduate students in the fields of ocean and marine engineering and naval architecture and associated fields will find the book useful.
















NASA SP.


Book Description